New Nickel Superalloy ABD-900AM Designed for Crack-Free Metal 3D…

April 27, 2026July 14, 2020 by Peter Gedeon

In past decades, additive manufacturing (AM) technologies introduced new possibilities for direct manufacturing of complex parts with costs and lead times

Categories News, Projects & Models Tags 3d-printed-alloys, abd-900am, additive-manufacturing-materials, crack-free-printing, high-performance-alloys, metal-additive-manufacturing, nickel-superalloy Leave a comment

About 3D Put

3D Put is your source for the latest in 3D printing news, tutorials, and innovations. We curate and deliver cutting-edge content from across the 3D printing ecosystem.

Quick Links

  • 3D Printer Comparison
  • 3D Printer Filament Settings (Verified + Practical)
  • 3D Printing News, Reviews & Comparison Tools
  • About Us
  • Affiliate Disclosure
  • Contact Us
  • Cookie policy
  • Disclaimer
  • DMCA & Copyright Policy
  • News
  • Privacy Policy
  • Terms of Service

Latest 3D Printer Reviews

  • Best PETG 3D Printing Settings Guide: Temperature, Speed, and Cooling for Strong Prints
  • Best 3D Printers Under $500: 2026 Comparison Guide
  • QIDI Max4 vs Sovol SV04: Full Specs Comparison & Buyer’s Guide
  • QIDI Max4 vs Flashforge Creator 3: Full Comparison
  • Sovol SV07 vs Sovol SV08: Full Specs Comparison & Buyer’s Guide
Privacy PolicyCookie Policy© 2026 3D PUT • Built with GeneratePress
Manage Cookie Consent
We use technologies like cookies to store and/or access device information. We do this to improve browsing experience and to show (non-) personalized ads. Consenting to these technologies will allow us to process data such as browsing behavior or unique IDs on this site. Not consenting or withdrawing consent, may adversely affect certain features and functions.
Functional cookies Always active
The technical storage or access is strictly necessary for the legitimate purpose of enabling the use of a specific service explicitly requested by the subscriber or user, or for the sole purpose of carrying out the transmission of a communication over an electronic communications network.
Preferences
The technical storage or access is necessary for the legitimate purpose of storing preferences that are not requested by the subscriber or user.
Statistics
The technical storage or access that is used exclusively for statistical purposes. The technical storage or access that is used exclusively for anonymous statistical purposes. Without a subpoena, voluntary compliance on the part of your Internet Service Provider, or additional records from a third party, information stored or retrieved for this purpose alone cannot usually be used to identify you.
Marketing
The technical storage or access is required to create user profiles to send advertising, or to track the user on a website or across several websites for similar marketing purposes.
  • Manage options
  • Manage services
  • Manage {vendor_count} vendors
  • Read more about these purposes
View preferences
  • {title}
  • {title}
  • {title}